End Mill Selection by Material: Aluminium, Graphite, CFRP and Steel
November 19, 2026 · Exactalloy
What is the best end mill for aluminum?
For aluminum, a 3-flute end mill with a high helix and polished flutes is the usual starting point. The polished surface stops soft aluminium from welding to the edge, which is the most common cause of poor finish. Uncoated or ZrN-coated tools usually beat AlTiN here because AlTiN contains aluminium and increases built-up edge. Run high spindle speed with strong chip evacuation, either flood coolant or MQL. For deep slots where chip room matters more than finish, drop to a single-flute cutter.
Which cutter should I use for graphite electrodes?
Graphite is abrasive rather than gummy, so the tool fails by wear, not by built-up edge. Use a diamond-coated (CVD) carbide tool with a low rake angle and a sharp, honed edge. Machine dry with high spindle speed and strong dust extraction; coolant turns graphite dust into a conductive slurry that damages machines and electronics. Expect tool life measured in electrodes rather than hours, and keep a wear log so you can replace tools before the edge rounds and starts burning the workpiece.
Can I mill carbon fiber with a standard end mill?
You can, but a standard end mill will delaminate the top and bottom plies and wear out quickly. CFRP needs a diamond-coated cutter with a compression or burr geometry so the cutting forces point inward on both faces. Use high spindle speed with low feed per tooth, clamp the laminate rigidly, and extract dust at the cut line. Edges that look fine often hide subsurface cracks, so inspect a scrap piece under magnification before committing a production batch.
What end mill should I use for titanium?
Titanium work-hardens and conducts heat poorly, so the heat goes into the edge. Use a sharp, uncoated or thin-coated carbide tool with a low helix, run low surface speed with a high feed per tooth, and never let the tool rub. Flood coolant is essentially mandatory, and it must be chlorine-free. Keep radial engagement moderate and climb mill. If you dwell or take tiny cuts, the surface hardens and the next pass destroys the edge.
Best cutter for hardened steel above 50 HRC?
Use a solid carbide end mill with an AlTiN or TiAlN coating and a high helix, run at low surface speed with a small radial depth of cut and a rigid, short-overhang setup. Hard milling removes the need for EDM in many mould cavities, but it leaves no margin for chatter: any vibration shows up as chipping on the cutting edge. Start conservative, verify with a single test cut, and increase feed before you increase speed.
Why does my cutter grab and squeal in copper and brass?
Soft, ductile metals grab when the edge rubs instead of cutting. The usual fixes are a higher rake angle, polished flutes, fewer flutes for more chip room, and enough feed per tooth to keep the edge biting. A worn or chipped edge will rub even with correct parameters, so check the edge under a magnifier first. In brass, avoid zero-rake tools that were designed for steel; they push material instead of shearing it.
How do I stop stainless steel from work hardening?
Keep the tool cutting, never dwelling. Climb milling, a sharp edge, a feed per tooth high enough to stay under the hardened layer, and copious coolant all matter. If a previous operation already hardened the surface, take a deeper pass that gets under the hard skin rather than a light spring pass that skates on it. Stainless also responds badly to re-cutting chips, so chip evacuation is part of the cutting strategy, not an afterthought.
Send your material, operation and existing parameters — an application engineer replies with a tool suggestion and, if useful, a trial-cut sample.